Broad estimates put the cost of corrosion to 1 to 4 % of GNP in the USA.  Whilst an accurate figure would be elusive to even the most rigorous rational, it is fair to say that repairing the consequences of corrosion is a costly business. Brass and austenitic stainless steel are widely used in engineering applications to convey liquids, such as water, or for pressurised applications, such as heat exchangers, steam generating equipment and pipework. As such, stress corrosion cracking can result in catastrophic, and costly, failures of this equipment. 

WHAT IS STRESS CORROSION CRACKING?

Stress corrosion cracking is a specific type of corrosion that often causes failures of engineering components.  Stress corrosion cracking occurs over time, with little readily apparent evidence of the degradation of the metal.  In addition, it occurs at stresses much lower than those required to produce a spontaneous failure due to overload (i.e. below the yield strength and often at normal service stresses). 

brass plumbing valve that failed due to stress corrosion cracking
A brass plumbing valve that failed due to stress corrosion cracking. The failure of the valve resulted in an escape of water and damage to a property.

SIGNS OF STRESS CORROSION CRACKING

Branched cracking is a common characteristic of stress corrosion cracking. When viewed at high magnification the fracture surface of a component that has failed due to stress corrosion cracking has a faceted and granular appearance (Photograph 2 below).  In contrast to this the fracture surface of a component that has failed due to a ductile overload failure typically has a dimpled appearance (Photograph 3 below). The facets and granular appearance actually reveal the small individual crystals (grains) that comprise the microstructure of the majority of engineering metals. 

A scanning electron micrograph showing the faceted and granular appearance of the fracture surface of a brass plumbing component that has failed due to stress corrosion cracking.
A scanning electron micrograph showing the dimpled appearance of the fracture surface of a brass component that has failed due to ductile overload.

SOURCES OF STRESS

A susceptible material, a tensile (pulling) stress and a specific corrosive species all need to be present simultaneously for stress corrosion cracking to occur. The stress can be from two sources:

  1. The first source of stress is from an applied stress. Applied stresses are those produced by service, such as the water pressure within a pipe, stresses produced by assembly of the item or the weight hanging from a fixture. 
  2. The second source of stress is from residual stress in the material. To some extent residual stresses are present in all materials and are often produced by relatively rapid cooling from elevated temperatures during manufacture. 

 

REDUCING THE LIKELIHOOD OF STRESS CORROSION CRACKING

Examples, of known species that cause stress corrosion cracking and the metals they affect are:

Specific Chemical Species

1.  Aqueous (water based) chloride, bromide and iodide solutions

2.  Aqueous chloride solutions

3.  Nitrate, hydroxide and carbonate/bicarbonate solutions

4.  Ammonia (and ammonia containing chemicals such as urea) and nitrates

Affected Metal(s)

1.  Aluminium and titanium alloys

2.  Austenitic stainless steels and magnesium alloys

3.  Carbon steels

4.  Brasses.  Brass is principally an alloy of copper and zinc

 

ABOUT THE AUTHOR

Neville Tranter started investigating mechanical failures in 2005.  Since then he has investigated the failure of a wide range of components, systems and structures; from medical devices such as stents and prosthesis, to bulk storage tanks, drilling Derrick and oil well drilling equipment, through aerospace and rail components, plumbing systems and many things in between. His background in Metallurgy makes him ideally placed to understand the design of equipment, the materials they are made out of, manufacturing processes used to produce them, service life and how these factors can result in failure. 

Share This

Follow us

Visit us on LinkedIn and YouTube to stay up to date with our latest content.